Aldehyde Resins(CF-A81、CF-A101)

General Description:

l      CF-A81 and CF-A101 are decolored aldehyde resins and can be applied in a wide range of coatings, and have excellent effects in increasing the anti-yellowing, coating glossiness and hardness, especially suitable for preparation of universal color pastes.

Properties:

Test Items

Unit

CF-A81

CF-A101

Test Method

Softening point

℃

90~105

106~120

ISO 4625

Colourity

Gardner color scale

≤1

≤1

ISO 4630

Acidity value

mgKOH/g

≤3

≤3

ISO 3682

Hydroxyl value

mgKOH/g

about 40

about 40

ISO 4629

Density(20℃)

g/cm3

1.1

1.1

DIN 53479

Features and Applications:

l      Aldehyde resins can be mixed with N/C, alcoholic acids or PU, chlorinated resin copolymer, and plasticizers for forming transparent or colored paints, which are applicable to the coating on wooden articles, metal and paper.

l      Aldehyde resins solutions have low viscosity and good fluidity. Besides they can increase the degree of cure of paints as well as the thickness, glossiness, hardness and anti-yellowing of the coating film.

l      Aldehyde resins are insoluble in aliphatic hydrocarbon solvents, and thus are applicable to gasoline-proof paints.

l      Aldehyde resins can be used in baking varnish formation. Neither odors are not given out nor are glossiness affected during baking process. 5% addition can increase the hardness from 1H to 3H, with good bending resistance.

Advantages of Aldehyde resins against Polyketone resins & Maleic resins:

l      Lighter color;

l      Better anti-aging and anti-yellowing performance;

l      Better fluidity, lower solution viscosity, and higher degree of cure;

l      Allow better solubility of N/C in mixture solvents;

l      Better flexibility;

l      Simpler dissolving and easier operation;

l      Faster drying.

Aldehyde resins apply to UV coatings, should pay attention to:

l      First, do formula aging test in the UV system:If the UV specimen baked in an80℃oven  over four hours, and then be put into gel, then the aldehyde resin can't be used, and should be replaced;After eight hours without gel, the aldehyde resin can be used.

l      If aldehyde resin is dissolved or dispersed in high temperature, the product maybe easy to gel. You should cool it and then make products.